Abiurana-branca vs East Indian Satinwood
Pouteria caimito against Chloroxylon swietenia. Every number below names the publication it came from.
| Property | Abiurana-branca | East Indian Satinwood |
|---|---|---|
| Janka hardness | 2,608 lbfLPF/SFB Madeiras Brasileiras | 2,600 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 56.8 lb/ft³LPF/SFB Madeiras Brasileiras | 61.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 23,042 lb/in²LPF/SFB Madeiras Brasileiras | 16,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.33 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.02 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 11,919 lb/in²LPF/SFB Madeiras Brasileiras | 10,030 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 14.5%LPF/SFB Madeiras Brasileiras | — |
| Tangential / radial ratio(lower is better) | 1.77LPF/SFB Madeiras Brasileiras | 1.29Chudnoff 1984, Tropical Timbers of the World (AH-607) |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- East Indian Satinwood moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.8, so it is the safer choice for a wide flat panel.
- Abiurana-branca carries 40% more load in bending, which matters for a shelf or a rail.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.