Wood movement calculator
Estimate how a board’s width changes as its wood moisture content changes. This method covers moisture contents from 6% to 14%.
Use wood moisture content from a suitable meter or a separate equilibrium-moisture estimate. These percentages are not the relative humidity of the air. Both values must be between 6 and 14.
Radial is perpendicular to growth rings, approximately the width direction of quartersawn boards. Tangential follows the rings, approximately the width direction of flatsawn boards.
Estimated width change
Orientation scenarios: +0.183 in to +0.263 in. This is the range between radial and tangential estimates, not a statistical confidence interval.
- Radial direction
- +0.183 in
- Final width: 24.183 in
- Tangential direction
- +0.263 in
- Final width: 24.263 in
Positive values mean expansion; negative values mean contraction. Individual boards and intermediate grain angles can differ. Use the estimate to plan construction that allows movement.
Data and calculation
Black walnut: green-to-oven-dry radial shrinkage 5.5%; tangential shrinkage 7.8%. These are source inputs, not seasonal movement percentages.
- Shrinkage source: USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3 · public domain.
The coefficient is derived from published shrinkage using USDA Wood Handbook 2021, Chapter 13, equations 13–2 and 13–3. The model assumes a fiber saturation point of 30% for this species and uses a coefficient referenced to 10% moisture content.
This is an approximate width estimate for the stated moisture range. It does not model warping, along-grain movement, or the clearances required by a specific joint. Missing, unsourced, or estimated shrinkage inputs do not produce a result.