Data sources and licences

This site holds 1785 species. 571 carry a published Janka test from a laboratory. 1212 carry a Janka value estimated from density, and 1687 carry at least one estimated value of any kind. Every estimate is marked on the page where it appears.

Sources

SourceLicenceSpecies
USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain1673
GWDD v2.2 (Fischer et al. 2026)CC BY 4.01234
USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-11apublic domain1212
USDA FIA REF_SPECIESpublic domain1181
Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain346
LPF/SFB Madeiras BrasileirasCC BY 4.0221
USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain115
USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain113
USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain80
USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain77
manual map (regional variant)public domain22
USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-4bpublic domain1

What this site refuses to publish

Many wood property numbers on the web trace back to one commercial database that reserves all rights to them. Wikipedia's Janka table cites that database in most of its rows, and the "wood datasets" on code-sharing sites are copies of it. None of those numbers appear here.

The result is a smaller database with a document behind every row. Where no laboratory tested a species, this site prints "no published test" rather than a borrowed figure.

Take the data

The compiled dataset is available as CSV and JSON. Public-domain values stay public domain. Values from a CC BY source keep their attribution requirement, which the source column records for each row.