The strongest woods
Ranked by modulus of rupture, which is the stress a beam carries at the moment it breaks. Strength and hardness are different properties. A hard wood can be brittle, and a strong wood can dent.
| # | Wood | MOR (lb/in²) | |
|---|---|---|---|
| 1 | African Blackwood | 31,000 lb/in² | |
| 2 | Jarana | 30,170 lb/in² | |
| 3 | Kaneelhart | 29,900 lb/in² | |
| 4 | Curupay | 29,290 lb/in² | |
| 5 | Aromata | 28,600 lb/in² | |
| 6 | Afina | 28,200 lb/in² | |
| 7 | Marishballi | 27,700 lb/in² | |
| 8 | Macawood | 27,600 lb/in² | |
| 9 | Sapucaia | 27,540 lb/in² | |
| 10 | Miraúba | 27,309 lb/in² | |
| 11 | Bulletwood | 27,300 lb/in² | |
| 12 | Pau-santo | 27,238 lb/in² | |
| 13 | RosadinhoPeltogyne paniculata | 27,138 lb/in² | |
| 14 | Abiurana-seca | 27,109 lb/in² | |
| 15 | IpêTabebuia sp | 26,697 lb/in² | |
| 16 | Casca-preciosa | 26,668 lb/in² | |
| 17 | IngáInga paraensis | 26,540 lb/in² | |
| 18 | Manbarklak | 26,500 lb/in² | |
| 19 | Wamara | 26,370 lb/in² | |
| 20 | Muirapixuna | 26,227 lb/in² | |
| 21 | Brush Box | 26,200 lb/in² | |
| 22 | Demerara Greenheart | 26,200 lb/in² | |
| 23 | Eveuss | 26,000 lb/in² | |
| 24 | Belian | 25,810 lb/in² | |
| 25 | Dina | 25,800 lb/in² | |
| 26 | MaçarandubaManilkara huberi | 25,560 lb/in² | |
| 27 | Ipe | 25,400 lb/in² | |
| 28 | East African Olive | 25,300 lb/in² | |
| 29 | Maçarandubarana | 25,232 lb/in² | |
| 30 | Ipê-amarelo | 25,176 lb/in² | |
| 31 | Black Cabbage-Bark | 25,000 lb/in² | |
| 32 | Casuarina | 25,000 lb/in² | |
| 33 | AbiuranaPouteria egregia | 24,919 lb/in² | |
| 34 | Greenheart | 24,900 lb/in² | |
| 35 | UrucuranaSloanea nitida | 24,877 lb/in² | |
| 36 | Jatobá / jutaí-do-campo | 24,635 lb/in² | |
| 37 | Uxirana | 24,635 lb/in² | |
| 38 | Jataipeba | 24,614 lb/in² | |
| 39 | MaçarandubaManilkara sp. | 24,593 lb/in² | |
| 40 | IpêHandroanthus serratifolius = Tabebuia serratifolia | 24,549 lb/in² | |
| 41 | Azobe | 24,500 lb/in² | |
| 42 | Cumaru | 24,371 lb/in² | |
| 43 | Gangaw | 24,065 lb/in² | |
| 44 | Louro-amarelo | 24,010 lb/in² | |
| 45 | Difou | 24,000 lb/in² | |
| 46 | Angelim / angelim-rajado | 23,724 lb/in² | |
| 47 | SucupiraBowdichia nitida | 23,663 lb/in² | |
| 48 | Oba | 23,600 lb/in² | |
| 49 | AbiuranaPouteria anomala | 23,525 lb/in² | |
| 50 | Missanda | 23,500 lb/in² |