Which woods suit a cutting board?
Two questions decide a board, and they need different evidence. Does the wood hold up? That is a property question, and the numbers answer it. Is the wood safe against food? That is a health question, and no open source answers it species by species.
So this page does not certify anything. It ranks the woods that suit the job on their measured properties, then it shows whether a published occupational source reports an effect for each one. You make the call, and you can see what it rests on.
Suited, with no published report
8 woods. No published report is not the same as proven safe: most of the world's timbers have never been assessed.
| Wood | Janka | Availability |
|---|---|---|
| Keruing | 1,270 lbf | |
| Rubberwood | 915 lbf | |
| Merbau | 1,500 lbf | |
| Black cherry | 950 lbf | |
| African mahogany | 830 lbf | |
| Hackberry | 880 lbf | |
| Magnolia | 1,090 lbf | |
| Kapur | 1,230 lbf |
Suited, but a source reports an effect
32 woods suit the job on the numbers, and carry a report. Most reports describe breathing the dust while machining, not contact with a finished surface. Read the species page before you decide.
What the ranking uses
A Janka between about 900 and 1,500 lbf, so the board resists scarring without destroying a knife edge, and then the lowest volumetric shrinkage, so it moves least between a wet season and a dry one. The order also weighs how easily you can buy the wood, which is the one editorial judgement on this site.
Grain matters too, and this database holds no measure of it. A closed-grain wood traps less food than an open-grain one, which is the usual argument against red oak whatever its numbers say.