Wood Record

The densest woods

Ranked by air-dry density at 12% moisture content. Density drives most other properties: a dense wood is usually hard and strong, and it is always heavy to carry.

A wood denser than 1,000 kg/m³ sinks in water.

#WoodDensity (lb/ft³)
1Holywood87.1 lb/ft³*
2Lignum-vitae87.1 lb/ft³*
3Muirapixuna84.1 lb/ft³*
4African Blackwood83.0 lb/ft³
5Leadwood81.2 lb/ft³*
6Lignumvitae80.0 lb/ft³
7Pau-santo78.7 lb/ft³
8Partridgewood78.0 lb/ft³
9Verawood78.0 lb/ft³
10Ngis76.3 lb/ft³*
11Bridgotree75.4 lb/ft³*
12Casca-preciosa75.4 lb/ft³*
13Desert ironwood75.4 lb/ft³*
14Quebracho75.0 lb/ft³
15Letterwood74.0 lb/ft³
16Jatobá / jutaí-do-campo73.4 lb/ft³*
17Mangle73.4 lb/ft³*
18Oysterwood73.4 lb/ft³*
19Pracuúba-da-terra-firme73.4 lb/ft³*
20Rochefortia spinosa73.4 lb/ft³*
21Bluewood72.5 lb/ft³*
22IpêHandroanthus serratifolius = Tabebuia serratifolia72.5 lb/ft³*
23Aromata72.0 lb/ft³*
24Blackbead ebony71.5 lb/ft³*
25Mulga71.5 lb/ft³*
26Pani71.5 lb/ft³*
27Poison ash71.5 lb/ft³*
28Sea torchwood71.5 lb/ft³*
29Wild cinnamon71.5 lb/ft³*
30Aceitillo70.6 lb/ft³*
31Gray ironbark70.6 lb/ft³*
32Azobe70.0 lb/ft³
33Ipe70.0 lb/ft³
34Wamara70.0 lb/ft³
35Black ironbox69.7 lb/ft³*
36Uxirana69.7 lb/ft³*
37CocoboloDalbergia retusa69.0 lb/ft³
38Jucaro69.0 lb/ft³
39Abiurana-seca68.7 lb/ft³*
40Allspice68.7 lb/ft³*
41IngáInga sp68.7 lb/ft³*
42Siamese rosewood68.7 lb/ft³*
43Miraúba68.0 lb/ft³
44Belian68.0 lb/ft³
45Eveuss68.0 lb/ft³
46AbiuranaPouteria egregia67.7 lb/ft³*
47Caribbean princewood67.7 lb/ft³*
48Cercipo67.7 lb/ft³*
49Florida hopbush67.7 lb/ft³*
50Goncalo alves67.7 lb/ft³*