Wood weight calculator
Give a species and a board size. The calculator uses the published density for that species at 12% moisture content.
- Total weight
- 12.8 lb
- 1 board
- Board feet
- 4.00
- Density used
- 38.5 lb/ft³
The density above is the published air-dry figure for Black walnut. That page names the source.
A real board differs from the table. Moisture content moves the figure most: wood at 20% moisture weighs about 8% more than the same wood at 12%. Treat the result as a planning figure, not as a shipping weight.