Wood Record

The softest woods

Ranked by the Janka side hardness test, softest first. A soft wood carves with hand pressure, and it also dents against a fingernail.

"Softwood" is a botanical word for a conifer, and it does not mean the wood is soft. Several conifers on this list are harder than several hardwoods.

#WoodJanka (lbf)
1Balsa88 lbf
2Ceiba240 lbf
3Duru250 lbf
4Figueira / gameleira269 lbf
5Caucho313 lbf
6Trumpet-Wood320 lbf
7Northern white cedar320 lbf
8Burra-leiteira324 lbf
9Cananga330 lbf
10Western redcedar350 lbf
11Subalpine fir350 lbf
12Quaking aspen350 lbf
13Black cottonwood350 lbf
14Atlantic white cedar350 lbf
15Cajá359 lbf
16Mastate360 lbf
17Binuang362 lbf
18Leiteiro379 lbf
19Sugar pine380 lbf
20Okoume380 lbf
21Eastern white pine380 lbf
22Cuangare380 lbf
23Balsam fir380 lbf
24Jelutong390 lbf
25Engelmann spruce390 lbf
26Chicha400 lbf
27Bombax400 lbf
28White spruce410 lbf
29Noble fir410 lbf
30American basswood410 lbf
31Alstonia410 lbf
32Young-growth redwood420 lbf
33Western white pine420 lbf
34Caroba / parapará423 lbf
35Sajo425 lbf
36Pacific silver fir430 lbf
37Obeche430 lbf
38Eastern cottonwood430 lbf
39Urucu-da-mata437 lbf
40Marupá452 lbf
41Pulai460 lbf
42Ponderosa pine460 lbf
43Mexican cypress460 lbf
44Light red meranti460 lbf
45Magas462 lbf
46Fava-bolota / visgueiro463 lbf
47Incense cedar470 lbf
48Espave470 lbf
49Deglupta470 lbf
50White fir480 lbf