Abiurana vs Angico
Pouteria egregia against Peltogyne cf subsessilis. Every number below names the publication it came from.
| Property | Abiurana | Angico |
|---|---|---|
| Janka hardness | 2,950 lbfLPF/SFB Madeiras Brasileiras | 2,941 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 67.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 60.6 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 24,919 lb/in²LPF/SFB Madeiras Brasileiras | 22,971 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.55 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.28 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,901 lb/in²LPF/SFB Madeiras Brasileiras | 17,168 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.7%LPF/SFB Madeiras Brasileiras | 13.4%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.65LPF/SFB Madeiras Brasileiras | 1.75LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Abiurana carries 8% more load in bending, which matters for a shelf or a rail.
- Abiurana is the heavier of the two by 115 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.