Wood Record

Abiurana vs Aromata

Pouteria egregia against Clathrotropis spp-. Every number below names the publication it came from.

PropertyAbiuranaAromata
Janka hardness2,950 lbfLPF/SFB Madeiras Brasileiras2,960 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC67.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-972.0 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture24,919 lb/in²LPF/SFB Madeiras Brasileiras28,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.55 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.50 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength12,901 lb/in²LPF/SFB Madeiras Brasileiras13,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)15.7%LPF/SFB Madeiras Brasileiras11.9%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.65LPF/SFB Madeiras Brasileiras1.34Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Aromata moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.6, so it is the safer choice for a wide flat panel.
  • Aromata carries 15% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons