Pouteria guianensis against Diploon cuspidatum = Diploon venezuelana. Every number below names the publication it came from.
| Property | Abiurana | Abiurana-seca |
|---|---|---|
| Janka hardness | 2,921 lbfLPF/SFB Madeiras Brasileiras | 2,945 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 58.7 lb/ft³LPF/SFB Madeiras Brasileiras | 68.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 20,382 lb/in²LPF/SFB Madeiras Brasileiras | 27,109 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | — | 2.57 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 9,871 lb/in²LPF/SFB Madeiras Brasileiras | 13,982 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 13.3%LPF/SFB Madeiras Brasileiras | 15.7%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.76LPF/SFB Madeiras Brasileiras | 1.42LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Abiurana-seca moves more evenly. Its tangential-to-radial ratio is 1.4 against 1.8, so it is the safer choice for a wide flat panel.
- Abiurana-seca carries 33% more load in bending, which matters for a shelf or a rail.
- Abiurana-seca is the heavier of the two by 161 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.