Wood Record

Abiurana vs Angico

Pouteria guianensis against Peltogyne cf subsessilis. Every number below names the publication it came from.

PropertyAbiuranaAngico
Janka hardness2,921 lbfLPF/SFB Madeiras Brasileiras2,941 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.7 lb/ft³LPF/SFB Madeiras Brasileiras60.6 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture20,382 lb/in²LPF/SFB Madeiras Brasileiras22,971 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—2.28 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,871 lb/in²LPF/SFB Madeiras Brasileiras17,168 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.3%LPF/SFB Madeiras Brasileiras13.4%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.76LPF/SFB Madeiras Brasileiras1.75LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Angico carries 13% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons