Wood Record

Abiurana vs Tuturubá

Pouteria guianensis against Pouteria oblanceolata. Every number below names the publication it came from.

PropertyAbiuranaTuturubá
Janka hardness2,921 lbfLPF/SFB Madeiras Brasileiras2,923 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.7 lb/ft³LPF/SFB Madeiras Brasileiras59.9 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture20,382 lb/in²LPF/SFB Madeiras Brasileiras22,217 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity—2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,871 lb/in²LPF/SFB Madeiras Brasileiras11,293 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.3%LPF/SFB Madeiras Brasileiras13.8%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.76LPF/SFB Madeiras Brasileiras1.71LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Tuturubá carries 9% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons