Abiurana vs Abiurana
Pouteria sp against Pouteria egregia. Every number below names the publication it came from.
| Property | Abiurana | Abiurana |
|---|---|---|
| Janka hardness | 2,418 lbfLPF/SFB Madeiras Brasileiras | 2,950 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 57.4 lb/ft³LPF/SFB Madeiras Brasileiras | 67.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 22,516 lb/in²LPF/SFB Madeiras Brasileiras | 24,919 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.45 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.55 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,436 lb/in²LPF/SFB Madeiras Brasileiras | 12,901 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.2%LPF/SFB Madeiras Brasileiras | 15.7%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.64LPF/SFB Madeiras Brasileiras | 1.65LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Abiurana resists denting better. It tests 22% harder than Abiurana.
- Abiurana carries 11% more load in bending, which matters for a shelf or a rail.
- Abiurana is the heavier of the two by 165 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.