Abiurana-seca vs Kaneelhart
Diploon cuspidatum = Diploon venezuelana against Licaria spp.. Every number below names the publication it came from.
| Property | Abiurana-seca | Kaneelhart |
|---|---|---|
| Janka hardness | 2,945 lbfLPF/SFB Madeiras Brasileiras | 2,900 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Density at 12% MC | 68.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 27,109 lb/in²LPF/SFB Madeiras Brasileiras | 29,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Modulus of elasticity | 2.57 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 4.06 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Crushing strength | 13,982 lb/in²LPF/SFB Madeiras Brasileiras | 17,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Volumetric shrinkage(lower is better) | 15.7%LPF/SFB Madeiras Brasileiras | 12.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 |
| Tangential / radial ratio(lower is better) | 1.42LPF/SFB Madeiras Brasileiras | 1.46USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 |
What the numbers mean
- The two match on hardness, within 2%. Choose on movement or on appearance instead.
- Kaneelhart carries 10% more load in bending, which matters for a shelf or a rail.
- Abiurana-seca is the heavier of the two by 108 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain