Wood Record

Abiurana-seca vs Sucupira

Diploon cuspidatum = Diploon venezuelana against Bowdichia nitida. Every number below names the publication it came from.

PropertyAbiurana-secaSucupira
Janka hardness2,945 lbfLPF/SFB Madeiras Brasileiras2,903 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC68.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-959.9 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture27,109 lb/in²LPF/SFB Madeiras Brasileiras23,663 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.57 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.33 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength13,982 lb/in²LPF/SFB Madeiras Brasileiras13,536 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.7%LPF/SFB Madeiras Brasileiras12.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.42LPF/SFB Madeiras Brasileiras1.64LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Abiurana-seca moves more evenly. Its tangential-to-radial ratio is 1.4 against 1.6, so it is the safer choice for a wide flat panel.
  • Abiurana-seca carries 15% more load in bending, which matters for a shelf or a rail.
  • Abiurana-seca is the heavier of the two by 141 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons