Abiurana vs Abiurana
Pouteria anomala against Pouteria guianensis. Every number below names the publication it came from.
| Property | Abiurana | Abiurana |
|---|---|---|
| Janka hardness | 2,472 lbfLPF/SFB Madeiras Brasileiras | 2,921 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 56.2 lb/ft³LPF/SFB Madeiras Brasileiras | 58.7 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 23,525 lb/in²LPF/SFB Madeiras Brasileiras | 20,382 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.31 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | — |
| Crushing strength | 12,246 lb/in²LPF/SFB Madeiras Brasileiras | 9,871 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.2%LPF/SFB Madeiras Brasileiras | 13.3%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.49LPF/SFB Madeiras Brasileiras | 1.76LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Abiurana resists denting better. It tests 18% harder than Abiurana.
- Abiurana moves more evenly. Its tangential-to-radial ratio is 1.5 against 1.8, so it is the safer choice for a wide flat panel.
- Abiurana carries 15% more load in bending, which matters for a shelf or a rail.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.