Wood Record

Abiurana vs Matamatá

Pouteria anomala against Eschweilera coriacea. Every number below names the publication it came from.

PropertyAbiuranaMatamatá
Janka hardness2,472 lbfLPF/SFB Madeiras Brasileiras2,467 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC56.2 lb/ft³LPF/SFB Madeiras Brasileiras56.2 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture23,525 lb/in²LPF/SFB Madeiras Brasileiras19,002 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.31 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.11 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength12,246 lb/in²LPF/SFB Madeiras Brasileiras9,181 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.2%LPF/SFB Madeiras Brasileiras16.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.49LPF/SFB Madeiras Brasileiras1.71LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Abiurana moves more evenly. Its tangential-to-radial ratio is 1.5 against 1.7, so it is the safer choice for a wide flat panel.
  • Abiurana carries 24% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.