Celtis spp. against Olea hochstetteri. Every number below names the publication it came from.

PropertyAfrican CeltisEast African Olive
Janka hardness1,670 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,740 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC45.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture20,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)25,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.30 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.53 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength10,550 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)15.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Tangential / radial ratio(lower is better)1.86Chudnoff 1984, Tropical Timbers of the World (AH-607)—

What the numbers mean

  • East African Olive resists denting better. It tests 64% harder than African Celtis.
  • East African Olive carries 21% more load in bending, which matters for a shelf or a rail.
  • East African Olive is the heavier of the two by 160 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.