| Property | African ebony | East African Camphorwood |
|---|---|---|
| Janka hardness | 3,220 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 930 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 63.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 37.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 21,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 13,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | — | 1.44 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 9,350 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 7,590 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 20.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | — |
| Tangential / radial ratio(lower is better) | 1.17USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | — |
What the numbers mean
- African ebony resists denting better. It tests 246% harder than East African Camphorwood.
- African ebony carries 59% more load in bending, which matters for a shelf or a rail.
- African ebony is the heavier of the two by 416 kg/m³, which a reader building a door or a case should weigh.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.