African ebony vs Muhimbi

Diospyros spp. against Cynometra alexandri. Every number below names the publication it came from.

PropertyAfrican ebonyMuhimbi
Janka hardness3,220 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,975 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC63.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)54.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture21,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)21,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity—2.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength9,350 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)10,400 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)20.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—
Tangential / radial ratio(lower is better)1.17USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—

What the numbers mean

  • African ebony resists denting better. It tests 8% harder than Muhimbi.
  • African ebony is the heavier of the two by 144 kg/m³, which a reader building a door or a case should weigh.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.