Wood Record

Amora / amoreira vs Courbaril

Maclura tinctoria against Hymenaea courbaril. Every number below names the publication it came from.

PropertyAmora / amoreiraCourbaril
Janka hardness2,385 lbfLPF/SFB Madeiras Brasileiras2,350 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC56.8 lb/ft³LPF/SFB Madeiras Brasileiras56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture22,259 lb/in²LPF/SFB Madeiras Brasileiras19,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.83 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.16 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength12,488 lb/in²LPF/SFB Madeiras Brasileiras9,510 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)9.4%LPF/SFB Madeiras Brasileiras12.7%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.84LPF/SFB Madeiras Brasileiras1.89USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Amora / amoreira carries 15% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons