Wood Record

Amora / amoreira vs Demerara Greenheart

Maclura tinctoria against Ocotea rodiaei. Every number below names the publication it came from.

PropertyAmora / amoreiraDemerara Greenheart
Janka hardness2,385 lbfLPF/SFB Madeiras Brasileiras2,360 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC56.8 lb/ft³LPF/SFB Madeiras Brasileiras66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture22,259 lb/in²LPF/SFB Madeiras Brasileiras26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.83 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.04 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength12,488 lb/in²LPF/SFB Madeiras Brasileiras13,040 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)9.4%LPF/SFB Madeiras Brasileiras17.1%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.84LPF/SFB Madeiras Brasileiras1.09Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Demerara Greenheart moves more evenly. Its tangential-to-radial ratio is 1.1 against 1.8, so it is the safer choice for a wide flat panel.
  • Demerara Greenheart carries 18% more load in bending, which matters for a shelf or a rail.
  • Demerara Greenheart is the heavier of the two by 147 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.