Angelim-amargoso vs Balsamo
Vatairea sericea against Myroxylon balsamum. Every number below names the publication it came from.
| Property | Angelim-amargoso | Balsamo |
|---|---|---|
| Janka hardness | 2,167 lbfLPF/SFB Madeiras Brasileiras | 2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 56.2 lb/ft³LPF/SFB Madeiras Brasileiras | 58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 19,323 lb/in²LPF/SFB Madeiras Brasileiras | 20,130 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.43 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 10,525 lb/in²LPF/SFB Madeiras Brasileiras | 11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 13.9%LPF/SFB Madeiras Brasileiras | 10.0%Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Tangential / radial ratio(lower is better) | 1.87LPF/SFB Madeiras Brasileiras | 1.63Chudnoff 1984, Tropical Timbers of the World (AH-607) |
What the numbers mean
- The two match on hardness, within 2%. Choose on movement or on appearance instead.
- Balsamo moves more evenly. Its tangential-to-radial ratio is 1.6 against 1.9, so it is the safer choice for a wide flat panel.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.