Wood Record

Angelim-amargoso vs Faveira-amargosa

Vatairea sericea against Vatairea paraensis. Every number below names the publication it came from.

PropertyAngelim-amargosoFaveira-amargosa
Janka hardness2,167 lbfLPF/SFB Madeiras Brasileiras2,174 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC56.2 lb/ft³LPF/SFB Madeiras Brasileiras62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture19,323 lb/in²LPF/SFB Madeiras Brasileiras21,519 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.18 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength10,525 lb/in²LPF/SFB Madeiras Brasileiras11,280 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.9%LPF/SFB Madeiras Brasileiras14.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.87LPF/SFB Madeiras Brasileiras2.04LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Faveira-amargosa carries 11% more load in bending, which matters for a shelf or a rail.
  • Faveira-amargosa is the heavier of the two by 97 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.