Wood Record

Angelim / angelim-rajado vs Bulletwood

Zygia racemosa = Marmaroxylon racemosum against Manilkara bidentata. Every number below names the publication it came from.

PropertyAngelim / angelim-rajadoBulletwood
Janka hardness3,177 lbfLPF/SFB Madeiras Brasileiras3,190 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC61.8 lb/ft³LPF/SFB Madeiras Brasileiras66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture23,724 lb/in²LPF/SFB Madeiras Brasileiras27,300 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.38 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.45 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength11,478 lb/in²LPF/SFB Madeiras Brasileiras11,640 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)15.2%LPF/SFB Madeiras Brasileiras16.9%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.58LPF/SFB Madeiras Brasileiras1.49USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Bulletwood carries 15% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons