Angelim / angelim-rajado vs Maçaranduba
Zygia racemosa = Marmaroxylon racemosum against Manilkara sp.. Every number below names the publication it came from.
| Property | Angelim / angelim-rajado | Maçaranduba |
|---|---|---|
| Janka hardness | 3,177 lbfLPF/SFB Madeiras Brasileiras | 3,228 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 61.8 lb/ft³LPF/SFB Madeiras Brasileiras | 66.8 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 23,724 lb/in²LPF/SFB Madeiras Brasileiras | 24,593 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.38 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.02 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,478 lb/in²LPF/SFB Madeiras Brasileiras | 11,961 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.2%LPF/SFB Madeiras Brasileiras | 16.4%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.58LPF/SFB Madeiras Brasileiras | 1.40LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 2%. Choose on movement or on appearance instead.
- Maçaranduba is the heavier of the two by 80 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.