Wood Record

Angelim-vermelho vs Belian

Dinizia excelsa against Eusideroxylon zwageri. Every number below names the publication it came from.

PropertyAngelim-vermelhoBelian
Janka hardness3,045 lbfLPF/SFB Madeiras Brasileiras3,020 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC66.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-968.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture22,758 lb/in²LPF/SFB Madeiras Brasileiras25,810 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.46 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.65 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength12,417 lb/in²LPF/SFB Madeiras Brasileiras13,620 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)14.5%LPF/SFB Madeiras Brasileiras—
Tangential / radial ratio(lower is better)1.67LPF/SFB Madeiras Brasileiras1.74Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Belian carries 13% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons