Wood Record

Angelim-vermelho vs Cabreúva-parda

Dinizia excelsa against Myrocarpus frondosus. Every number below names the publication it came from.

PropertyAngelim-vermelhoCabreúva-parda
Janka hardness3,045 lbfLPF/SFB Madeiras Brasileiras3,075 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC66.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-957.4 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture22,758 lb/in²LPF/SFB Madeiras Brasileiras22,359 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.46 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.19 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength12,417 lb/in²LPF/SFB Madeiras Brasileiras12,460 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)14.5%LPF/SFB Madeiras Brasileiras11.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.67LPF/SFB Madeiras Brasileiras1.59LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Angelim-vermelho is the heavier of the two by 151 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons