Angico vs Uxirana
Peltogyne cf subsessilis against Vantanea parviflora. Every number below names the publication it came from.
| Property | Angico | Uxirana |
|---|---|---|
| Janka hardness | 2,941 lbfLPF/SFB Madeiras Brasileiras | 2,948 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 60.6 lb/ft³LPF/SFB Madeiras Brasileiras | 69.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 22,971 lb/in²LPF/SFB Madeiras Brasileiras | 24,635 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.28 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.55 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 17,168 lb/in²LPF/SFB Madeiras Brasileiras | 12,531 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 13.4%LPF/SFB Madeiras Brasileiras | 17.6%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.75LPF/SFB Madeiras Brasileiras | 1.26LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Uxirana moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.7, so it is the safer choice for a wide flat panel.
- Uxirana is the heavier of the two by 146 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.