Wood Record

Anoerá-ferro vs Leche Perra

Acioa sp against Helicostylis tomentosa. Every number below names the publication it came from.

PropertyAnoerá-ferroLeche Perra
Janka hardness2,683 lbfLPF/SFB Madeiras Brasileiras2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC60.6 lb/ft³LPF/SFB Madeiras Brasileiras55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture20,326 lb/in²LPF/SFB Madeiras Brasileiras22,800 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.12 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.86 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength10,768 lb/in²LPF/SFB Madeiras Brasileiras12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)15.1%LPF/SFB Madeiras Brasileiras14.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.82LPF/SFB Madeiras Brasileiras1.70Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Leche Perra carries 12% more load in bending, which matters for a shelf or a rail.
  • Anoerá-ferro is the heavier of the two by 89 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons