Aromata vs Tuturubá
Clathrotropis spp- against Pouteria oblanceolata. Every number below names the publication it came from.
| Property | Aromata | Tuturubá |
|---|---|---|
| Janka hardness | 2,960 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,923 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 72.0 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 59.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 28,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 22,217 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.50 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 13,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 11,293 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 11.9%Chudnoff 1984, Tropical Timbers of the World (AH-607) | 13.8%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.34Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.71LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Aromata moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.7, so it is the safer choice for a wide flat panel.
- Aromata carries 29% more load in bending, which matters for a shelf or a rail.
- Aromata is the heavier of the two by 194 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.