Aromata vs Uxirana

Clathrotropis spp- against Vantanea parviflora. Every number below names the publication it came from.

PropertyAromataUxirana
Janka hardness2,960 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,948 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC72.0 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-969.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture28,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)24,635 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity3.50 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.55 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength13,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,531 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)11.9%Chudnoff 1984, Tropical Timbers of the World (AH-607)17.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.34Chudnoff 1984, Tropical Timbers of the World (AH-607)1.26LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Aromata carries 16% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.