Azobe vs Rhodesian-Teak
Lophira alata against Baikiaea plurijuga. Every number below names the publication it came from.
| Property | Azobe | Rhodesian-Teak |
|---|---|---|
| Janka hardness | 3,350 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2,990 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 70.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 24,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 12,220 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.47 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 1.23 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 12,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 9,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 17.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | — |
| Tangential / radial ratio(lower is better) | 1.31USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | — |
What the numbers mean
- Azobe resists denting better. It tests 12% harder than Rhodesian-Teak.
- Azobe carries 100% more load in bending, which matters for a shelf or a rail.
- Azobe is the heavier of the two by 224 kg/m³, which a reader building a door or a case should weigh.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.