Balsamo vs Breu-manga

Myroxylon balsamum against Tetragastris altissima. Every number below names the publication it came from.

PropertyBalsamoBreu-manga
Janka hardness2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,169 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)58.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,130 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)19,529 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.43 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.08 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,079 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)10.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)13.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.63Chudnoff 1984, Tropical Timbers of the World (AH-607)1.96LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Balsamo moves more evenly. Its tangential-to-radial ratio is 1.6 against 2.0, so it is the safer choice for a wide flat panel.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.