Wood Record

Balsamo vs Carne D'Anta

Myroxylon balsamum against Maytenus spp.. Every number below names the publication it came from.

PropertyBalsamoCarne D'Anta
Janka hardness2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,240 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)54.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture20,130 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)18,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.43 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.41 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)10.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Tangential / radial ratio(lower is better)1.63Chudnoff 1984, Tropical Timbers of the World (AH-607)1.93Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 2%. Choose on movement or on appearance instead.
  • Balsamo moves more evenly. Its tangential-to-radial ratio is 1.6 against 1.9, so it is the safer choice for a wide flat panel.
  • Balsamo carries 11% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.