Wood Record

Balsamo vs Louro-faia

Myroxylon balsamum against Roupala montana. Every number below names the publication it came from.

PropertyBalsamoLouro-faia
Janka hardness2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,169 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)61.3 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,130 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)22,957 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.43 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.46 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,032 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)10.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)18.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.63Chudnoff 1984, Tropical Timbers of the World (AH-607)1.95LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Balsamo moves more evenly. Its tangential-to-radial ratio is 1.6 against 2.0, so it is the safer choice for a wide flat panel.
  • Louro-faia carries 14% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons