Wood Record

Balsamo vs Muhuhu

Myroxylon balsamum against Brachylaena hutchinsii. Every number below names the publication it came from.

PropertyBalsamoMuhuhu
Janka hardness2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,190 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture20,130 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)16,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.43 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.46 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)10,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)10.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Tangential / radial ratio(lower is better)1.63Chudnoff 1984, Tropical Timbers of the World (AH-607)—

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Balsamo carries 24% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons