Myroxylon balsamum against Euxylophora paraensis. Every number below names the publication it came from.

PropertyBalsamoPau-amarelo
Janka hardness2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,168 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)50.6 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture20,130 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)17,566 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.43 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.92 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)10,092 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)10.0%Chudnoff 1984, Tropical Timbers of the World (AH-607)11.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.63Chudnoff 1984, Tropical Timbers of the World (AH-607)1.36LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Pau-amarelo moves more evenly. Its tangential-to-radial ratio is 1.4 against 1.6, so it is the safer choice for a wide flat panel.
  • Balsamo carries 15% more load in bending, which matters for a shelf or a rail.
  • Balsamo is the heavier of the two by 119 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.