Barrote vs Black Cabbage-Bark
Tetragastris panamensis against Lonchocarpus spp.. Every number below names the publication it came from.
| Property | Barrote | Black Cabbage-Bark |
|---|---|---|
| Janka hardness | 2,693 lbfLPF/SFB Madeiras Brasileiras | 2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 57.4 lb/ft³LPF/SFB Madeiras Brasileiras | 52.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 17,843 lb/in²LPF/SFB Madeiras Brasileiras | 25,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 1.98 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 3.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 9,373 lb/in²LPF/SFB Madeiras Brasileiras | 12,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 14.9%LPF/SFB Madeiras Brasileiras | — |
| Tangential / radial ratio(lower is better) | 1.96LPF/SFB Madeiras Brasileiras | — |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Black Cabbage-Bark carries 40% more load in bending, which matters for a shelf or a rail.
- Barrote is the heavier of the two by 87 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.