Wood Record

Barrote vs Brazilian rosewood

Tetragastris panamensis against Dalbergia nigra. Every number below names the publication it came from.

PropertyBarroteBrazilian rosewood
Janka hardness2,693 lbfLPF/SFB Madeiras Brasileiras2,720 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC57.4 lb/ft³LPF/SFB Madeiras Brasileiras64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture17,843 lb/in²LPF/SFB Madeiras Brasileiras19,000 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.98 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.88 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength9,373 lb/in²LPF/SFB Madeiras Brasileiras9,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)14.9%LPF/SFB Madeiras Brasileiras8.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.96LPF/SFB Madeiras Brasileiras1.59USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Brazilian rosewood moves more evenly. Its tangential-to-radial ratio is 1.6 against 2.0, so it is the safer choice for a wide flat panel.
  • Brazilian rosewood is the heavier of the two by 107 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.