Wood Record

Belian vs Mururé

Eusideroxylon zwageri against Brosimum gaudichaudii. Every number below names the publication it came from.

PropertyBelianMururé
Janka hardness3,020 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)3,036 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC68.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)56.8 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture25,810 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)19,941 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.65 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.06 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength13,620 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,165 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—14.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.74Chudnoff 1984, Tropical Timbers of the World (AH-607)1.82LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Belian carries 29% more load in bending, which matters for a shelf or a rail.
  • Belian is the heavier of the two by 179 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.