Belian vs Rhodesian-Teak
Eusideroxylon zwageri against Baikiaea plurijuga. Every number below names the publication it came from.
| Property | Belian | Rhodesian-Teak |
|---|---|---|
| Janka hardness | 3,020 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,990 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 68.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 25,810 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 12,220 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.65 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.23 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 13,620 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 9,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | — | — |
| Tangential / radial ratio(lower is better) | 1.74Chudnoff 1984, Tropical Timbers of the World (AH-607) | — |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Belian carries 111% more load in bending, which matters for a shelf or a rail.
- Belian is the heavier of the two by 192 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.