Lonchocarpus spp. against Dalbergia nigra. Every number below names the publication it came from.

PropertyBlack Cabbage-BarkBrazilian rosewood
Janka hardness2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,720 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC52.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture25,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)19,000 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity3.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.88 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength12,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)—8.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)—1.59USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Black Cabbage-Bark carries 32% more load in bending, which matters for a shelf or a rail.
  • Brazilian rosewood is the heavier of the two by 194 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons