Black Cabbage-Bark vs Castanha-de-cutia
Lonchocarpus spp. against Acioa edulis. Every number below names the publication it came from.
| Property | Black Cabbage-Bark | Castanha-de-cutia |
|---|---|---|
| Janka hardness | 2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,696 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 52.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 64.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 25,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 21,847 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.36 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 11,748 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | — | 17.5%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | — | 1.28LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Black Cabbage-Bark carries 14% more load in bending, which matters for a shelf or a rail.
- Castanha-de-cutia is the heavier of the two by 207 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.