Black Cabbage-Bark vs Goiabão
Lonchocarpus spp. against Chrysophyllum lucentifolium = Pouteria pachycarpa. Every number below names the publication it came from.
| Property | Black Cabbage-Bark | Goiabão |
|---|---|---|
| Janka hardness | 2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,646 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 52.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 58.1 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 25,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 22,999 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.41 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 11,357 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | — | 16.5%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | — | 1.81LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 2%. Choose on movement or on appearance instead.
- Black Cabbage-Bark carries 9% more load in bending, which matters for a shelf or a rail.
- Goiabão is the heavier of the two by 97 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.