Wood Record

Black Cabbage-Bark vs Leche Perra

Lonchocarpus spp. against Helicostylis tomentosa. Every number below names the publication it came from.

PropertyBlack Cabbage-BarkLeche Perra
Janka hardness2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC52.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture25,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)22,800 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity3.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.86 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength12,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)—14.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—1.70Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Black Cabbage-Bark carries 10% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.