Black Cabbage-Bark vs Maçarandubarana
Lonchocarpus spp. against Chrysophyllum prieurii. Every number below names the publication it came from.
| Property | Black Cabbage-Bark | Maçarandubarana |
|---|---|---|
| Janka hardness | 2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,725 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 52.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 61.8 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 25,000 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 25,232 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 10,810 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | — | 20.3%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | — | 1.69LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Maçarandubarana is the heavier of the two by 157 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.