Brazilian rosewood vs Caraipé

Dalbergia nigra against Licania octandra. Every number below names the publication it came from.

PropertyBrazilian rosewoodCaraipé
Janka hardness2,720 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,754 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-961.3 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture19,000 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b23,355 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.88 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.47 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b12,090 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)8.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-417.4%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.59USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.95LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Brazilian rosewood moves more evenly. Its tangential-to-radial ratio is 1.6 against 2.0, so it is the safer choice for a wide flat panel.
  • Caraipé carries 23% more load in bending, which matters for a shelf or a rail.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.