Brazilian rosewood vs Castanha-de-cutia
Dalbergia nigra against Acioa edulis. Every number below names the publication it came from.
| Property | Brazilian rosewood | Castanha-de-cutia |
|---|---|---|
| Janka hardness | 2,720 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2,696 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 64.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 19,000 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 21,847 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 1.88 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2.36 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 9,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 11,748 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 8.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 17.5%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.59USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 1.28LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Castanha-de-cutia moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.6, so it is the safer choice for a wide flat panel.
- Castanha-de-cutia carries 15% more load in bending, which matters for a shelf or a rail.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.